Casting defects and methods of detection
Answers
Answered by
1
Fluorescent powder testing only detects surface cracks and flaws but is more effective and economical than radiographic testing. In general, dye-penetranttechniques identify defects on the surface of the casting and do not detect internal porosity or shrinkage that is not open to the surface.