describe the extraction of lanthanide from monazite
Answers
Answered by
1
Answer:
Explanation:
Acid cracking. The original process for "cracking" monazite so as to extract the thorium and lanthanide content was to heat it with concentrated sulfuric acid to temperatures between 120 and 150 °C for several hours.