explain intergranular corrosion and galvanic corrosion. Also gives way of minimizing them​

Answers

Answered by shradhakumariyadav
0

Answer:

Intergranular corrosion can be prevented through: Use low carbon (e.g. 304L, 316L) grade of stainless steels. Use stabilized grades alloyed with titanium (for example type 321) or niobium (for example type 347). Titanium and niobium are strong carbide- formers