Plaster of Paris is prepared by heating gypsum at 373 K. On heating, it loses water molecules and becomes calcium sulphate hemihydrate (CaSO4. 1/2 H2O) which is called Plaster of Paris.
#HOPE IT HELPS........!!!!!!!
Answered by
1
Explanation:
on heating gypsum at 373 k,it loses water molecules and becomes calcium sulphate hemihydrate(caso4.1/2H2O).
CaSO4.2H2O= CaSO4.1/2H2O
(on heating at 373k)