in case of Under reinforced section which element fails first
Answers
Answered by
1
Reinforced concrete beam sections in which the steel reaches yield strain at loads lower than the load at which the concrete reaches failure strain are called under-reinforced sections. Every singly reinforced beam should be designed as under-reinforced sections because this section gives enough warning before failure.
hope it helps you
mark me as brainliest please
Answered by
4
Answer:
Reinforced concrete beam sections in which the steel reaches yield strain at loads lower than the load at which the concrete reaches failure strain are called under-reinforced sections. Every singly reinforced beam should be designed as under-reinforced sections because this section gives enough warning before failure.