In zinc plating the rate of deposit per minute at 4 Ampere/dm^2 will be nearly?
Answers
Answered by
0
am using ammonium chloride zinc plating (barrel plating). For getting 3-4 microns it takes 2-3 hrs. We are plating to the fasteners of different types.