Incomplete Penetration. Incomplete penetration happens when your filler metal and base metal aren't joined properly, and the result is a gap or a crack of some sort. ...
Incomplete Fusion. ...
Undercutting. ...
Slag Inclusions. ...
Flux Inclusions. ...
Porosity. ...
Cracks. ...
✓ Hot cracks:
Incomplete Penetration. Incomplete penetration happens when your filler metal and base metal aren't joined properly, and the result is a gap or a crack of some sort. ...
Incomplete Fusion. ...
Undercutting. ...
Slag Inclusions. ...
Flux Inclusions. ...
Porosity. ...
Cracks. ...
✓ Hot cracks:
Answered by
5
Porosity
lack of fusion and cold lap
excessive spatter
concave and convex weld beads
crater crackes
lack of fusion and cold lap
excessive spatter
concave and convex weld beads
crater crackes