Chemistry, asked by SaiShivanee6277, 10 months ago

Write name of defects observed in brass

Answers

Answered by monulovemonu
2

Answer:

The casting step of leaded brass billet may be including some defects such as surface and lead clustering defects, zinc segregation, cavities with porosity and non-metallic contaminations due to the effects of recycle rate, impurities and casting parameters.

Answered by priyaag2102
1

DEFECTS OBSERVED IN BRASS

Explanation:

Brass Defect:-

A defect is an irregularity produced during the metal production process that is undesired and cannot be  tolerated. These defects are divided into two types depending upon the process of production.  

A. Hidden Defects

These defects occur during casting stage of brass. These defects are hidden / undersurface and usually  become evident in subsequent machining processes which lead to the rejection of finished products. There are five  main categories of casting defects;

a) Shrinkage defects

b) Gas porosity

c) Mold material defects

d) Pouring metal defects

e)  Metallurgical defects

B. Surface Defects

Following are the common types of surface defects;

i. Blister; This form when air traps in the material and develops envelops which appears on one or  both sides of the strip consisting of swellings.

ii. Scaly; This defect develops as a result of peeling / bursting of blister during Hot or Cold rolling.

iii. Red strains; This defect occurs when Un-dissolved copper appears on the upper surface of the  strip.

iv. Cracks; Such type of defects is due to breakage of grains & improper mixing of material during  lead rolling mixing.

Similar questions