34) pitting corrosion occurs due to
formation of
Answers
Answered by
0
Answer:
The more conventional explanation for pitting corrosion is that it is an autocatalytic process. Metal oxidation results in localized acidity that is maintained by the spatial separation of the cathodic and anodic half-reactions, which creates a potential gradient and electromigration of aggressive anions into the pit.