According to me,the lower critical temperature of high carbon steel
lower critical temp below which pearlite starts to form.(723°C)
Explanation:
The lower critical temp below which pearlite starts to form.(723°C)
Heating is carried out (20°C) above the upper critical temperature of steel in case of hypo-eutectoid steel and same degree above the lower critical point of steel in case of hyper- eutectoid steel.
The most commonly used operations of heat treatment for iron and steel are: 1. Annealing
2. Normalising
3. Hardening
4. Tempering
5. Carburising (Case-Hardening)
6. Cyaniding
7. Nitriding
8. Induction Hardening
9. Flame-Hardening.
The former consists of ferrite and pearlite while the latter consists of pearlite and cementite.
Similar questions
Computer Science,
6 months ago
Social Sciences,
6 months ago
Chemistry,
11 months ago
Political Science,
11 months ago
Math,
1 year ago
Physics,
1 year ago
Science,
1 year ago