Physics, asked by yatiksha3508, 1 year ago

What is the ratio of vertical etch rate to horizontal etch rate

Answers

Answered by Anonymous
6

The etching process that involves using liquid chemicals or etchants to take off the substrate material is called wet etching. In the plasma etching process, also known as dry etching, plasmas or etchant gases are used to remove the substrate material. ... On the other hand, wet etching is only a chemical process.

__________________

cRAZY pRINCE

Answered by Anonymous
0

wet etching is the answer...