what are the various types of casting defects?
explain in detail
Answers
Answered by
1
Answer:
A casting defect is an undesired irregularity in a metal casting process. ... They are broken down into five main categories: gas porosity, shrinkage defects, mould material defects, pouring metal defects, and metallurgical defects.
pls mark as brainliest answer
Explanation:
Answered by
3
- Gas Porosity. Pinholes. Blowholes. Open Holes.
- Shrinkage Defects. Open. Closed. Warping.
- Mold Material Defects. Cuts and Washes. Swells. Drops. Metal Penetration. Rat Tails. Fusion. Run Out.
- Pouring Metal Defects. Cold Shot. Cold Shut. Misrun.
- Metallurgical Defects. Hot Tears. Hot Spots. Slag inclusion.